Why Do Transverse Streaks Appear During Coating?
Home » Blogs » Why Do Transverse Streaks Appear During Coating?

Why Do Transverse Streaks Appear During Coating?

Views: 0     Author: Site Editor     Publish Time: 2026-11-17      Origin: Site

Inquire

facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
kakao sharing button
sharethis sharing button
Why Do Transverse Streaks Appear During Coating?

A practical troubleshooting guide for coating lines

 

Transverse streaks can originate in the coating head, drying section, web-tension system, or winding stage. The fastest way to narrow down the cause is not to dismantle the line—it is to observe how the streak spacing responds to a controlled change in line speed.

image.png

Coating surface showing visible transverse streaking.

Start with a Speed-Reduction Test

Use a simple speed test to split the investigation into two paths: defects synchronized with web movement and defects generated by a fixed-frequency source.

Run a roll that shows transverse streaks and measure the distance between adjacent streaks. Then reduce the line speed to approximately one-third of its normal value and run a short section. Measure the spacing again.

· If the spacing increases: The defect is likely synchronized with web movement. Check components linked to the web, such as the traction roller, feed pump, and coating-roll drive.

· If the spacing remains almost unchanged or becomes shorter: A fixed-speed component or vibration source is more likely. Check the motor, fan, independently driven rollers, and other sources of periodic vibration.

No disassembly is required. A short length of defective material, a tape measure, and about ten minutes can reduce the potential search area from the entire production line to roughly half.

image.png

Figure 1. Diagnostic flowchart for identifying speed-synchronized and fixed-frequency sources of transverse streaks.

Coating Head: Check the Die Gap and Roller Runout

There are two key areas to investigate at the coating head: whether the coating liquid is supplied steadily, and whether the geometry of the coating interface remains accurate.

Slot-Die Coating: Check for Feed-Pressure Pulsation

With slot-die coating, transverse streaks are often caused not by the die body itself, but by instability in the liquid supply.

The reciprocating action of a piston pump can generate pressure pulses. The streak frequency may correspond directly to the operating rate of the piston units. For a rotary pump, the pulse frequency follows the pump speed (RPM).

A low-cost diagnostic test is to install a pulsation dampener in the feed line. As a temporary test, a section of flexible plastic hose can also replace a rigid metal pipe. The hose expands and contracts slightly, absorbing part of the pressure pulsation.

If the streaks become less pronounced, the feed system is strongly implicated.

Periodic pressure changes in the vacuum chamber can also move the coating meniscus back and forth. Inspect the chamber for leaks and check vacuum-pump stability. Use a vacuum gauge to see whether the pressure fluctuates in a regular pattern.

Micro-Gravure and Comma Coating: Measure Roller Runout

For micro-gravure and comma-bar coating, roller-surface runout should be one of the first suspects.

If the runout of a micro-gravure roll exceeds 5 μm, the coating thickness may develop periodic wave-like variations. The higher the line speed, the closer the transverse streaks may appear.

New rollers are sometimes installed immediately after delivery without a runout check. Do not assume that a new roller is automatically within tolerance—measure it before installation.

The inspection logic for a comma blade is similar, but the blade itself also needs attention. Check blade-edge straightness, installation angle, and whether dried coating has accumulated on the back of the blade.

If the blade-pressure sensor reading must be continually increased to maintain coating performance, this is a sign that the blade may need replacement.

Slight vibration in the backing-roll bearings can also cause defects. Measure radial runout with a dial indicator and replace components that exceed the specified tolerance rather than relying on another trial run.

Drying Section: Is the Airflow Fluctuating—or the Temperature?

Transverse streaks in the drying section should not be attributed simply to “too much air.” Separate the investigation into three possible causes: airflow pulsation, air-nozzle design, and temperature-control oscillation.

Airflow Pulsation and Nozzle Design

If the air nozzles use an array of round holes rather than a slot design, high air velocity may disturb the coating surface and create transverse streaks.

This type of defect can be particularly noticeable at the beginning of a reduced-speed drying section. At that point, the coating temperature is approaching the air temperature, the surface viscosity is low, and the coating is least resistant to airflow disturbance.

Temperature-Control Oscillation

Temperature-control instability can be harder to identify than airflow problems.

On one water-based coating line, transverse streaks appeared at intervals of 5–8 cm. The coating head was inspected thoroughly, and the tension settings were calibrated section by section, but neither showed an obvious problem.

A surface-temperature check with an infrared thermometer near the dryer exit revealed that the streak positions corresponded to a temperature-fluctuation zone in the third oven section.

The hot-air temperature fluctuated by ±8°C. At a line speed of 20 m/min, the coating passed through that zone in just 1.5 seconds. During this short interval, the temperature could change by 16°C, abruptly changing the surface-drying rate and producing streaks.

The identified root cause was ageing PID temperature-control parameters. At low speed, thermal inertia averaged out the fluctuations. When the line speed increased, the defect became visible.

When checking the dryer, do not look only at the temperature setpoint. Review the recorded temperature trend. A stable setpoint does not guarantee a stable actual temperature.

Web Tension and Winding: Resonance Has a Measurable Frequency

Tension-related transverse streaks can occur when periodic excitation coincides with the natural frequency of the web-handling system. Calculate the frequencies instead of relying on intuition.

In flotation drying sections or long-span web paths, airflow fluctuations are not necessarily smooth sine waves. A total airflow fluctuation of ±10% can generate periodic excitation in the range of 5–15 Hz, while the natural frequency of a roll-to-roll system is typically in the range of 8–22 Hz.

When these frequency ranges overlap, the amplitude of tension fluctuation can increase by a factor of 4–6.

Check Roller Eccentricity and Transmission Clearance

The contribution of drive rollers is easy to underestimate. Roller eccentricity above 0.05 mm or transmission-roller clearance above 0.1 mm can generate periodic tension pulses with an amplitude of ±3 N.

Review the Winding Taper-Tension Setting

In the winding section, check the taper-tension setting. Tension should decrease as roll diameter increases. If it does not, or if a soft substrate is run under excessive tension when it should use lower tension and a larger taper, cross-web thickness variations may accumulate along the roll length.

Do Not Assume Higher Tension Means Greater Stability

The operating limits in this section matter. In the low-tension range of 5–10 N, each 1 N increase in tension can raise the critical instability speed by 8–10%. Above 15 N, however, the improvement drops sharply to 2–3%. Increasing tension further may reduce the substrate's yield strength and create a cycle in which tighter control actually makes the system less stable.

When PET film approaches a tensile limit of 25 N, the risk of web breakage can rise from 0.5% to 20%. The material loss and cleanup cost from a single web break can reach the equivalent of RMB 100,000.

Before adjusting tension, identify the operating range of the specific substrate. Knowing the limits is more useful than simply recording a setpoint.

Track Process Boundaries—not Just Machine Settings

Recurring transverse streaks are often not isolated equipment failures. They may indicate that a process boundary has gradually been crossed.

Add three columns to the SOP or shift log: defect rate, downtime per shift, and filter-element replacement interval. Reviewing these three indicators together can help reveal the nature of the problem.

For example, if the streak defect rate for a batch rises suddenly from 2% to 8%, the filter replacement interval shortens from two weeks to five days, and downtime increases, the likely cause may be agglomerated particles or sediment in the slurry rather than the equipment.

If the defect rate rises in step with the number of shutdowns and restarts, inspect the wet-film condition of the first product after restart. Check the parallelism of the backing roll after it has been opened and closed, whether the comma blade's zero position has shifted, and whether residual air remains in the feed line.

There is no universal number of operating hours for replacing a comma blade. Monitor the pressure trend. If pressure must be increased continuously to maintain coating performance, the blade may need to be replaced. Do not wait until transverse streaks appear.

Set a Routine Runout Check for Micro-Gravure Rolls

Measure micro-gravure roll runout with a dial indicator once a month. If runout exceeds 5 μm, take corrective action. This measurable limit is more reliable than a purely experience-based judgment.

A Practical Troubleshooting Checklist

· First, run the speed-reduction test. Compare streak spacing at normal speed and at approximately one-third speed.

· Then inspect the coating head. Check feed-pressure pulsation, vacuum stability, roller runout, blade condition, and backing-roll bearings.

· Next, review the drying section. Check airflow disturbance, nozzle design, and actual temperature trends—not just setpoints.

· Then evaluate web handling. Compare excitation frequencies with system natural frequencies; inspect roller eccentricity, clearance, and winding taper tension.

· Finally, review process records. Track defect rate, shift downtime, filter replacement intervals, and restart conditions.

A reliable investigation follows the evidence from one section to the next. Start with the simplest speed test, measure rather than guess, and use process trends to catch instability before it develops into a recurring quality problem.

Since 2016 we committed to building brandof “TAILAI”,  “integrity and sustainable development”will always be our company policy.

QUICK LINKS

PRODUCTS

CONTACT US

  +86-1370-550-8718
  aozhenggang01@gmail.com
   Zhenggang Ao
  Xingye Road and Yuanzhuang Road,         Wuyi Industrial park,Nanqiao district,            Chuzhou 239001,Anhui ,China
Copyright © 2026 CHUZHOU TAILAI IMPORT&EXPORT TRADING CO.,LTD.